APA:
Roth, Jože, Bizjak, Milan, Kosec, Ladislav (2000). Temperaturna nestabilnost mikrostrukturnih sestavin v zlitinah Ag-Te in Ag-Se.
Materiali in tehnologije, volume 34, issue 3/4, str. 147-150.
URN:NBN:SI:DOC-4CLI82V8 from http://www.dlib.si
MLA:
Roth, Jože, Bizjak, Milan, Kosec, Ladislav. "Temperaturna nestabilnost mikrostrukturnih sestavin v zlitinah Ag-Te in Ag-Se."
Materiali in tehnologije volume 34. issue 3/4 (2000) str. 147-150.
<http://www.dlib.si/?URN=URN:NBN:SI:DOC-4CLI82V8>