<Record><identifier xmlns="http://purl.org/dc/elements/1.1/">URN:NBN:SI:DOC-OEHP1PFU</identifier><date>2015</date><creator>Jaber, Hassanen Latef</creator><creator>Marashi, Seyed Pirooz Hoveida</creator><creator>Pouranvari, Majid</creator><relation>documents/doc/O/URN_NBN_SI_doc-OEHP1PFU_001.pdf</relation><relation>documents/doc/O/URN_NBN_SI_doc-OEHP1PFU_001.txt</relation><format format_type="issue">4</format><format format_type="volume">49</format><format format_type="type">article</format><format format_type="extent">str. 579-585</format><identifier identifier_type="COBISSID">1162154</identifier><identifier identifier_type="ISSN">1580-2949</identifier><identifier identifier_type="URN">URN:NBN:SI:doc-OEHP1PFU</identifier><language>eng</language><publisher>Inštitut za kovinske materiale in tehnologije</publisher><source>Materiali in tehnologije</source><rights>InC</rights><subject language_type_id="eng">advanced high-strength steel</subject><subject language_type_id="eng">failure mode</subject><subject language_type_id="slv">način</subject><subject language_type_id="slv">porušitev</subject><subject language_type_id="eng">resistance spot welding</subject><subject language_type_id="slv">uporovni točkasti zvar</subject><subject language_type_id="slv">visokotrdnostno jeklo</subject><title>critical fusion-zone size ensuring the pull-out failure mode</title><title>DP780 dual-phase-steel spot welds</title><title>kritična velikost staljene cone, ki zagotavlja porušenje z izpuljenjem</title><title>Točkasti zvari jekla DP780 z dvofazno strukturo</title></Record>